EVA or TPU: a buyer guide to price, application and supply in 2026

2026-11-19 · XSMATECH material guide

EVA or TPU comparison

Buyers often ask us to quote “clear flexible film” and then choose on price alone. EVA and TPU are not interchangeable, and the price gap – roughly 17 CNY/kg against 25 CNY/kg – buys specific performance. Here is how the two materials actually differ in 2026.

1. Price and what drives it

EVA film, 0.05-1.0 mm: about 17 CNY/kg. Base resin: EVA foam and film grade, currently 10,900 CNY/t spot (Yangzi-BASF, 19 Nov 2026), down 5.6% in two weeks as solar encapsulation demand slowed. Resin is roughly two thirds of our price; the rest is calendering, packing and margin.

TPU film, 0.05-2.0 mm, 85A-95A: about 25 CNY/kg. TPU is a block copolymer of BDO, MDI and adipate polyol. All three moved up through the first half of 2026 – BDO on plant turnarounds, MDI on tight overseas supply – and TPU followed. Since September the market has been range-bound rather than trending, which is why our TPU quote has been stable while EVA has moved.

The practical point: EVA quotes move with one feedstock complex; TPU quotes move with three. If you need price stability for a season-long programme, TPU has been the steadier number this year, even though it is the more expensive one.

2. Where each one wins

EVA wins on: food contact and children’s products (plasticiser-free, low odour), cost-sensitive volume, soft-touch lamination, and packaging windows where the part does not flex hard in service.

TPU wins on: abrasion and flex fatigue (shoe uppers, soles, sports goods), transparency with weldability (bag windows, inflatables), oil and low-temperature resistance (industrial and automotive), and any part that gets a drop test or a chemical exposure test.

A simple filter we use with customers: if the finished part must pass a mechanical test, it is TPU. If it must pass a food-contact or cost test, it is EVA.

3. Competitive landscape

EVA: the high-volume grades are dominated by large Chinese producers – Yangzi-BASF, Sinopec affiliates, and the newer solar-grade lines at Sierbang and Lianhong. Film-grade converting is fragmented, with many small and mid-size calenderers; quality varies mostly in gel count, thickness tolerance and odour. That fragmentation is where a factory like ours competes: consistent gauge control and a documented food-contact file.

TPU: upstream is concentrated (BASF, Covestro, Lubrizol internationally; Wanhua, Huafeng, Miracll domestically). Film converting is again fragmented, but the entry barrier is higher than EVA because customers usually demand test data – hydrolysis resistance, yellowness after UV, adhesion after welding. A converter without those files cannot sell into footwear or automotive.

4. What we hold and how we quote

We run PVC, EVA, TPU and PE on eight calendering and blown-film lines in Yiwu, with 1,062 tonnes in stock across 94 grades. Stock colours ship in three days; production colours run 1-2 tonnes in 10-15 days. We load from Yiwu or Guangzhou and quote CIF from either port, and we can supply REACH, RoHS and EN 71-3 documentation with the sample.

If you send us the part drawing or a photo of the finished product, we will tell you which of the two materials it should be, and quote that one – rather than quoting both and letting price decide.

Contact: Oven Pan · admin@xsmatech.com · WhatsApp +86 138 2608 3558 · xsmatech.com

Prices are our current ex-works bands, subject to grade, colour and quantity. Feedstock references: Zhejiang Plastics Association spot releases (EVA, PVC) and Dalian Commodity Exchange settlement, 19 Nov 2026.